Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 495N - PS-I - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 495N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Styrolution® PS 495N is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 9.5 cm³/10min ISO 1133
Temperatura 200 °C -
Carga 5 kg -
Densidad de fusión 935 kg/m³ -
Conductibilidad termica de fusión 0.165 W/(m K) -
Calor especifico de la masa 2290 J/(kg K) -
Temperatura de expulsión 88 °C -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 2000 MPa ISO 527
Esfuerzo de fluencia 26 MPa ISO 527
Alarg. en límite elástico 1.5 % ISO 527
Alarg. nominal a rotura 40 % ISO 527
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 130 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 17 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 85 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 89 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 88.5 °C ISO 306
Coef.de expansión térmica lineal, paralelo 100 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 3.0 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 2.5 - IEC 62631-2-1
Constante dieléctrica, 1MHz 2.5 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 4 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 4 E-4 IEC 62631-2-1
Indice comparativo de linea de fuga 500 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1030 kg/m³ ISO 1183
Funciones
Viscosidad-velocidad de cizallamiento , Styrolution® PS 495N, PS-I, INEOS Styrolution
Tensión de cizalla-velocidad de cizalla , Styrolution® PS 495N, PS-I, INEOS Styrolution
Esfuerzo-alargamiento , Styrolution® PS 495N, PS-I, INEOS Styrolution
Módulo secante-alargamiento , Styrolution® PS 495N, PS-I, INEOS Styrolution
Volumen especifico-temperatura (pvT) , Styrolution® PS 495N, PS-I, INEOS Styrolution
Módulo a tensión-temperatura , Styrolution® PS 495N, PS-I, INEOS Styrolution
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características especiales
Alto impacto o modificado al impacto
Disponibilidad regional
Demás información
Moldeo por inyección
PROCESSING
injection molding, Melt temperature, range: 180 - 260 °C
injection molding, Melt temperature, recommended: 220 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 495N can be injection moulded under different conditions depending on machinery available and articles moulded. Mass temperature can be as high as 260°C. Polystyrol 495N is suitable for gas assisted injection moulding.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.